Expansion Rate: L:195; S:145.
|
Test Item |
Test Standard | Test Condition | Unit | Result |
| Hardness | ASTMD2240 | Test with Skin on | Shore Hardness C | 44 |
| Density | ASTMD792 | Archimedes Method | g/cm3 | 0.178 |
| Spring Back | GB/T6670-2008 | One-Meter Drop Ball | % | 48 |
| Tensile Strength |
ASTMD624 |
|
N/MM2 | 1.758 |
| Breaking Elongation | ASTMD412 |
|
% | 199 |
| Right-angle Tear | ASTMD624 |
|
N/MM | 6.5 |
| Compressive Deformation | ASTMD395 | 50% 50℃6H | % | 41.35 |
| Wear-resisting | GB3903.2 | 20MIN 5N | MM | 11,9 |